Skip to main content

Table 1 Histological evaluation format of cell and tissue response for implant material scoring

From: Fixation technique of biodegradable magnesium alloy suture anchor in the rotator cuff repair of the shoulder in a goat model: a technical note

Group

Control

Test

Implant material

Commercial Titanium

suture anchors

Innovative MgF2 ZK60

suture anchors

 

Observation period

Post-OP 3ms

Post-OP 3ms

Animal code

G24

G25

Area of interest

Infraspinatus tendon

Infraspinatus tendon

Section code

L shoulder

R shoulder

L shoulder

R shoulder

H&E stain

  

Polymorphonuclear cells

1

0

1

0

Lymphocytes

1

1

1

1

Plasma cells

0

0

0

0

Macrophages

1

0

1

0

Giant cells

0

1

0

0

Necrosis

0

0

1

0

SUB-TOTAL (x2)

6

4

6

2

Neovascularization

1

0

1

0

Fatty infiltrate

2

0

0

0

MT stain

  

Fibrosis

3

4

4

4

SUB-TOTAL

6

4

4

4

GROUP TOTAL

12

8

10

6

Averagea

20/2 = 10.0

16/2 = 8.0

 

Test-Control = 0.0, no reaction

No. Sites examined

2/2

2/2

  1. Post-OP 3 ms, 3 months postoperatively; H&E stain: hematoxylin and eosin; MT, Masson trichrome
  2. aUsed to determine reaction ranking shown below as he conclusion. A negative difference was recorded as zero