From: Articular cartilage generation applying PEG-LA-DM/PEGDM copolymer hydrogels
 | 60/40 (PEG-LA-DM/PEGDM) | 70/30 (PEG-LA-DM/PEGDM) | ||||||
---|---|---|---|---|---|---|---|---|
 | Time 0 Controlb | 6 weeks | 12 weeks | 18 weeks | Time 0 Control | 6 weeks | 12 weeks | 18 weeks |
Wet weight (mg) | 103.50 ± 4.10 | 91.35 ± 4.31 | 111.05 ± 4.59 | 117.90 ± 4.38 | 104.80 ± 8.06 | 100.35 ± 3.61 | 107.45 ± 2.57 | 114.30 ± 2.54 |
Volume (mm3) | 93.54 ± 1.21 | 86.09 ± 3.92 | 96.02 ± 3.89 | 104.55 ± 1.32 | 92.92 ± 4.64 | 91.87 ± 1.42 | 93.79 ± 1.38 | 102.85 ± 2.37 |
Water content (%) | 82.29 ± 3.78 | 79.01 ± 4.05 | 85.70 ± 2.45 | 86.09 ± 2.95 | 83.14 ± 3.87 | 80.07 ± 4.42 | 86.22 ± 3.17 | 85.61 ± 2.91 |